Home - Products - Crystal Growth Furnace - Czochralski (CZ) Crystal Growth Furnace for metals and oxides
The equipment is mainly used for scientific research to explore the crystal growth process, and can be used for the preparation of oxide single crystal and metal single crystal crystal, such as sapphire, GGG, YAG, LaAlO3, Si and Ge etc
Technical Parameters
Product Description:
The equipment is mainly used for scientific research to explore the crystal growth process, and can be used for the preparation of oxide single crystal and metal single crystal crystal, such as sapphire, GGG, YAG, LaAlO3, Si and Ge
Product Features:
1. Modular design, compact structure, beautiful appearance,
2. The side door is opened, the structure is exquisite, convenient, the movement is stable, and the loading and unloading is convenient
3· Touch screen + PLC control mode, high degree of automation, intuitive operation and powerful functions.
4· Dozens of sintering processes can be pre-stored in the touch screen, edited once, and directly called for use later, saving the trouble of editing the process multiple times, avoiding input errors and burning the product.
5· The sintering temperature, vacuum, and other data can be recorded in real time, and can also be started and stopped at any time to reduce useless data, and the data can be queried and exported and downloaded.
6· High sintering temperature, with graphite crucible, up to 1800 °C,
Main technical Parameters:
Product Model | KS-CGF-CZ400 czochralski growth furnace |
Total power | ≤15Kw, power supply voltage 3-phase 380V, 50Hz |
Cold ultimate vacuum degree | 6.7*10-3pa |
Maximum temperature | 1800°C heating power ≤10Kw single-phase 380V |
Rated temperature | room temperature ~ 1700°C |
Crucible size | Ф60×100mm (diameter × height,) |
Cavity size | Ф400*600mm (tentative) |
Temperature measurement system | tungsten polythermocouple |
Temperature control accuracy | ±1°C |
Lifting speed | slow lifting 0.8-50mm/h (servo control) |
The rotation speed of the lifting rod | 0.1-20r/min |
Lifting and lowering speed of the lift rod | 40mm/min |
Lifting stroke | ≤300mm |
Furnace charging pressure | ≤0.03MPa |